                              | EP75-1: Electrically conductive adhesive for a sensor in a biomarker detector | 
                             
                            
                               | 
                             
                            
                            
                              | Master Bond EP75-1 epoxy was used in the integration of a nanoparticle-sensitized printed flexible chemiresistor sensor on paper. This sensor, developed by researchers at SUNY Binghamton and SUNY Stony Brook, aims to detect chemical species as a lower-cost alternative to traditional semiconductor sensors. Learn more about how EP75-1 epoxy played a crucial role in advancing paper-based sensor technology.  | 
                             
                            
                               | 
                             
                            
                               | 
                             
                            
                            
                              | 
                                
                               | 
                             
                            
                           
                         | 
                       
                      
                         | 
                       
                     
                   | 
                 
               
             | 
           
          
             | 
           
         
       | 
     
   
  
   
  
    
      
        
          
            
              
                
                  
                    
                      
                         | 
                       
                      
                        
                          
                          
                          
                          
                          
                          
                            
                              
                                
                                  
                                    
                                    
                                      | Two Part Epoxy EP75-1 | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | Master Bond EP75-1 is a two part, graphite filled, electrically conductive epoxy for high performance bonding, sealing and coating.  | 
                                     
                                    
                                    
                                       | 
                                     
                                    
                                    
                                      | 
                                        
                                       | 
                                     
                                    
                                    
                                       | 
                                     
                                   
                                 | 
                               
                             
                           
                          
                          
                         
                         | 
                       
                     
                     |  
                   | 
                 
                  
                
               
             | 
           
         
       | 
     
   
  
  
  
   
  
    
      | 
        
       | 
     
    
      
        
          
             | 
           
          
            
              
              
              
 
              
              
                
                  | 