Supreme 11HT-LO Product Information

Supreme 11HT-LO Two Part Epoxy System

Two Component, Room Temperature Curing, High Temperature Resistant Epoxy Adhesive/Sealant for Service from -112°F to +400°F Featuring High Peel and High Shear Strength. Meets NASA Low Outgassing Specifications.

Supreme 3 Product Description

Supreme 3 One Part Epoxy

One Component, Low Temperature Heat Curing Epoxy Adhesive Featuring Both High Shear and High Peel Strength for Optimal Bonding Performance.

Supreme 30 Product Description

Supreme 30 Two Component Epoxy

Low Viscosity, Toughened Two Component Epoxy Adhesive For High Performance General Purpose Bonding.

Supreme 30AOHT Product Description

Supreme 30AOHT Two Part Epoxy

Toughened Thermally Conductive Electrically Insulating Two Component Epoxy System For High Performance General Purpose Bonding, Sealing and Casting Featuring Superior Flowability and High Temperature Resistance

Supreme 33 Product Information

Supreme 33 Two Part Epoxy

Two Component, Room Temperature Curing, Toughened Epoxy Adhesive/Sealant for High Temperature Bonding Applications Up To 425°F. Features Convenient Handling

Supreme 33CLV Product Information

Supreme 33CLV Two Part Epoxy

Two Component, Room Temperature Curing, Toughened Epoxy Adhesive/Sealant for High Temperature Bonding and Sealing. Offers High Shear and Peel Strength, Along With Convenient Handling.

Supreme 3AN Product Description

Supreme 3AN One Part Epoxy

One Component, Heat Curing Epoxy Adhesive, Sealant Featuring Both High Shear and High Peel Strength for Optimal Bonding Performance and Exceptionally High Thermal Conductivity

Supreme 3ANHT Product Information

Supreme 3ANHT One Part Epoxy

One Component, Heat Curing Epoxy Adhesive, Sealant Featuring Both High Shear and High Peel Strength for Optimal Bonding Performance and Exceptionally High Thermal Conductivity

Supreme 3AO Product Description

Supreme 3AO One Part Epoxy System

One Component, Thermally Conductive, Low Temperature Heat Curing Epoxy Adhesive Featuring Both High Shear and High Peel Strength for Optimal Bonding Performance.

Supreme 3AOHT Product Information

Supreme 3AOHT One Part Epoxy

One Component, Fast Curing, Toughened Epoxy for Bonding, Sealing and Coating Featuring Excellent Thermal Conductivity and Very Good Electrical Insulation Properties. Can Withstand Rigorous Thermal Cycling.