Distinct Master Bond formulations resist continuous, intermittent immersion, spillage, vapor exposure from specific organic and inorganic solvents. These ambient temperature, thermal curing and UV cure epoxy systems are designed for short term (30 days) and long term exposures. Products exhibit excellent bond strength between similar/dissimilar substrates including metals, ceramic, glass, plastic surfaces. Select grades have been developed to withstand heat aging and high stress in various solvent environments for indoor/outdoor usage. These 100% solid Master Bond compounds are available in liquid/paste viscosities and are easy to apply.
Master Bond Solvent Resistant Systems
From processing facilities to production plants to power stations, Master Bond solvent resistant adhesives, sealants and coatings are satisfying the needs of material and design engineers. Manufacturers of automotive, marine, military, agriculture, mining equipment, oil/gas processing components, electronic devices, scientific instruments depend on Master Bond for challenging adhesive bonding applications that require exposure to the following organic and inorganic solvents:
| Oxygenated Solvents | Hydrocarbon Solvents | Halogenated Solvents | Inorganic Solvents` | 
|---|---|---|---|
| Alcohols | Gasoline | Trichlorethylene | Water | 
| Methyl acetate | Hexane | Carbon tetrachloride | Surfacants | 
| Ketones | Benzene | Hycrochlorofluorocarbon | Detergents | 
| Esters | Toluene | Ethylene Dibromide | |
| Acetone | Xylene | 
Testing/evaluation should replicate actual usage conditions to confirm suitability of the epoxy adhesive, sealant, coating for your specific application.
Chemical Resistance Data for Master Bond Formulations
The graph below shows the weight change of EP41S-5 as a % versus time (number of weeks) when immersed in acetone:

The graph below shows the weight change of UV25 as a % versus time (number of weeks) when immersed in methylene chloride:

Master Bond's database of chemical immersion tests extends up to 10 years
Most Popular Solvent Resistant Polymer Systems
                        | 
                  
            EP41S-1HT Two component, ambient temperature curing system with excellent physical properties. Thermally stable. High compressive strength. Features extraordinary resistance to fuels, alcohols and organic solvents. Withstands 1,000 hours 85°C/85% RH. Service temperature range -60°F to +400°F. Moderate viscosity. Good electrical insulator.  | 
              
                        | 
                  
            EP45HT High performance adhesive/sealant/coating. Serviceable from -80°F to +500°F. Resists thermal cycling. Outstanding resistance to acids, bases, petrochemicals, water. 100% reactive. Cures at elevated temperatures. Good flow properties. Moderate viscosity. Excellent performance profile for long term exposures at 400°F to 450°F. Well suited for moderate sized electronic potting applications.  | 
              
                        | 
                  
            EP41S-5ND Black Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.  | 
              
                        | 
                  
            EP41S-5Med Excellent chemical resistance to solvents, bases, acids, alcohol and fuels. Withstands exposure to methylene chloride, phenol (10%) and nitric acid (30%). Well suited for coating tanks, pumps and vessels. Moderate viscosity with good flow properties. Can be used for potting/encapsulation. Formidable physical strength properties. Serviceable from -80°F to +450°F.  | 
              
                        | 
                  
            Supreme 42HT-2ND Black Non-drip epoxy paste, black in color, has outstanding temperature and chemical resistance. Superior toughness and thermal cycling capability. Meets low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superb electrical insulator. Service temperature range -80°F to +450°F.  | 
              
			      