Serviceable up to +500°F, EP13SPND-2 is a one part epoxy paste for structural bonding applications. This electrically insulative system has a non-drip application feature that delivers high tensile, tensile lap shear and compressive strength of over 8,000 psi, 3,000 psi and 18,000 psi, respectively.
It also offers superb dimensional stability and chemical resistance.