Two component, room temperature curing epoxy system for bonding, sealing, coating and encapsulation featuring a wide range of desirable properties

EP30-2 Two Part Epoxy Compound

Key Features

  • Extremely optically clear
  • Superb physical strength properties
  • Meets NASA low outgassing specifications
  • Cryogenic serviceability
  • Outstanding electrical properties
  • Withstands 1,000 hours 85°C/85% RH