Supreme 45HTAO Product Description | MasterBond.com

Two Component Toughened Thermally Conductive Epoxy Adhesive for High Performance Structural Bonding, Sealing and Coating

Supreme 45HTAO Two Part Epoxy

Master Bond Polymer Adhesive Supreme 45HTAO is a two component thermally conductive, electrically insulative epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitable for applications where long term exposure to temperatures from -78