Master Bond MasterSil 151Med was utilized by researchers in an implantable device for electrical nerve stimulation.
Two component, biocompatible silicone compound for potting and encapsulation
Key Features
- Meets USP Class VI specifications
- Passes ISO 10993-5 for cytotoxicity
- High flexibility
- Optically clear
- Electrically insulative
- Low viscosity