Moderate viscosity ethyl cyanoacrylate for medical device bonding applications

MB297Med-1 One Part Ethyl Cyanoacrylate Adhesive

Key Features

  • One component, no mix system
  • Meets USP Class VI specifications
  • Fast setting
  • Rapid fixture time