Master Bond EP30-2LB epoxy system blocks UV light while allowing the transmission of visible light.
This two part, optically clear compound meets NASA low outgassing specifications and features high optical clarity with a refractive index of 1.55.

Master Bond EP30-2LB epoxy system blocks UV light while allowing the transmission of visible light.
This two part, optically clear compound meets NASA low outgassing specifications and features high optical clarity with a refractive index of 1.55.