EP3HTS-LO is a fast curing, electrically conductive epoxy adhesive that is NASA low outgassing approved. It doesn’t require mixing, features an “unlimited” working life at room temperature and has a smooth thixotropic paste viscosity.
This infographic clearly presents all the product property details at a glance, including its amazingly low volume resistivity and high thermal conductivity.
![One Part, Silver Filled Epoxy Compound](/sites/default/files/igimages/OneComponentSilverFilledEpoxySystem.jpg)