Master Bond Product Search

439 products match

Two Component Epoxy EP62-1ND EP62-1ND

Cures rapidly at elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Shore D hardness 75-85. Thixotropic paste.

EP65 Two Component Epoxy EP65

Two component fast curing epoxy adhesive. Serviceable from -80°F to +300°F. Rapid setting times of 8-10 minutes. Excellent durability. High tensile lap shear strength. Superior moisture, chemical, creep, corrosion resistance.

EP65HT Two Component Epoxy EP65HT

Ultra fast curing two component epoxy adhesive. Rapid setup times and thermal stability. Cures quickly even in small masses. Serviceable from -60°F to +400°F. Tg is 125-130°C. NASA low outgassing certified. High tensile modulus. Superb electrical insulation properties. Vacuum compatibility. Available for use in gun dispenser.

EP65HT-1 Two Part Epoxy EP65HT-1

Two part, fast setting (3-5 minutes in 10-20 gram masses) room temperature curing epoxy. Serviceable from -60°F to +400°F. Tg of 125-130C. NASA low outgassing approved. Used by Boeing in various MRO applications. High tensile modulus. Excellent dimensional stability. Withstands 1,000 hours 85°C/85%RH. Can be applied with gun dispenser.

EP70CN

Two part, thermally stable epoxy adhesive formulated using a natural, renewable and sustainable ingredient. Features robust electrical insulation combined with lower exotherm enabling it to be used in a wide array of potting applications. Service temperature range is -80°F to +450°F.

Two component, highly flexible epoxy system EP72M4 EP72M4

Tough, resilient, room temperature curing epoxy adhesive. Resists exposure to vibration, impact and shock. Superior peel and shear strength.
Serviceable from -60°F to +250°F. Convenient one to one mix ratio weight or volume. Good chemical resistance. Superb electrical insulation properties.

Low viscosity, optically clear, two part epoxy adhesive EP88FL

Low viscosity, optically clear adhesive. Resistant to thermal cycling and thermal shock. Highly desirable Shore D hardness range. Bonds well to dissimilar substrates. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume.

EP90FR-H Two Part Epoxy EP90FR-H

Two component high strength flame retardant epoxy system. Meets stringent horizontal burn test portion of the FAR standard 14 CFR 25.853(a). Non-halogenated System. Forgiving one to one mix ratio by weight. Good electrical insulation. Serviceable from -60°F to +250°F. Low shrinkage.

EP90FR-HFL Two Part Epoxy EP90FR-HFL

Toughened epoxy system complies with FAR standard 14CFR 25.853(a) for flame retardancy. Bonding, sealing, coating, potting compound. Passes horizontal burn test specification. Withstands mechanical shock and vibration. Thermal cycling resistant. Non-halogenated type system. Bonds well to dissimilar substrates. Serviceable from -60°F to +250°F. Impressive electircal insulator.

EP90FR-V Two Part Epoxy System EP90FR-V

Two part epoxy passes vertical burn test portion of FAR standard 14 CFR 25.853(a) for flame retardancy. Passes Boeing standard BSS 7238, Revision C for low smoke and BSS 7239, Revision A for toxicity. Bonds well to variety of substrates. One to one mix ratio by weight. Moderate viscosity. Serviceable from -60°F to +250°F. Excellent electrical insulator. Non-halogenated system.