439 products match
Supreme 11HT-4 Two component, high strength epoxy adhesive. Serviceable for -100°F to +400°F. Excellent electrical insulation characteristics. Adheres well to similar/dissimilar substrates. Aramid fiber reinforcement for dimensional stability. Exceptional durability. 100 to 40 mix ratio by weight. Versatile cure schedules. |
|
Supreme 11HT-LO Room temperature curing epoxy adhesive has a convenient one to one mix ratio. High shear and peel strength. Toughened. NASA low outgassing approved. Stress cracking fatigue resistant. Serviceable from -100°F to +400°F. Withstands 1,000 hours 85°C/85% RH. Fast setting. Good flow. Easy to apply. |
|
Supreme 11HTLP High viscosity, two component, toughened epoxy adhesive/sealant. One to one mix ratio weight or volume. Favorable open time. Cure readily at room temperature. Outstanding toughness. High shear/peel strength. Resists impact, shock, thermal cycling. Serviceable from -100°F to +400°F. |
|
Supreme 11HTLV High peel and shear strength system. Convenient one to one mix ratio. Serviceable from -100°F to +350°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. Readily machinable. |
|
Supreme 11HTND High peel and shear strength system. Convenient one to one mix ratio with paste consistency. Serviceable from -112°F to +400°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. |
|
Supreme 11LV High peel and shear strength system. Convenient one to one mix ratio. Serviceable from -100°F to +250°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. Readily machinable. |
|
Supreme 17HT Master Bond Supreme 17HT is a one component toughened epoxy for bonding and sealing. It has a moderate viscosity system with good flow properties.The service temperature range is from -100°F to +550°F. |
|
Supreme 17HTMed Master Bond Supreme 17HTMed is a one component toughened epoxy for bonding and sealing that meets ISO 10993-5 for biocompatibility. It has a moderate viscosity system with good flow properties.The service temperature range is from -100°F to +550°F. |
|
Supreme 17HTND-2 Master Bond Supreme 17HTND-2 is a one component toughened epoxy for bonding and sealing. It is a paste system with good physical strength properties.The service temperature range is from -100°F to +550°F. |
|
Supreme 3 Storage stable one component heat curing epoxy adhesive. Versatile cure schedules. Electrically insulative. Durable system. Resists thermal cycling. Serviceable from -100°F to +250°F. |