556 products match
![]() |
Supreme 10AOHT-LO Thermally conductive and electrically insulative, one part epoxy adhesive. Superior toughness and dimensional stability. Bonds are resistant to thermal cycling and many chemicals. Serviceable from 4K to +400°F. NASA low outgassing approved. Withstands 1,000 hours 85°C/85% RH. Impressive physical strength properties. |
![]() |
Supreme 10HT One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance. |
![]() |
Supreme 10HTCL Single component toughened epoxy adhesive with good flow properties. Resistant to thermal cycling, mechanical vibration/shock. Tensile lap shear strength 2,800-3,000 psi. T-peel strength 25-30 pli. Cures in 60-75 minutes at 250°F, shorter times at higher temperatures. Successfully tested at 1,000 hours 85°C/85% RH. Serviceable from 4k to +400°F. |
![]() |
Supreme 10HTF-1 Fast curing one component thixotropic paste epoxy. Excellent bond strength. Superb toughness and durability. Viscosity remains constant with time. Solid chemical resistance. Reliable electrical insulator. Serviceable from 4k to +400°F. |
![]() |
Supreme 10HTFL Highly flexible, no mix adhesive. Offers outstanding peel strength. 100% reactive. Superior water and chemical resistance. Successfully tested for 1,000 hours 85°C/85% RH. Withstands rigorous thermal cycling. Serviceable from 4k to +350°F. |
Supreme 10HTLV One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance. |
|
![]() |
Supreme 11 High shear/peel strength epoxy adhesive. Two component system offers one to one mix ratio by weight or volume. Temperature range from -100°F to +300°F. Resists impact, thermal shock and stress cracking fatigue. Excellent long-term durability. Easy application. |
![]() |
Supreme 112 Potting, encapsulation, coating, sealing, impregnation compound. Low viscosity, long working life. Superior physical strength. Serviceable from -80°F to 550°F. |
![]() |
Supreme 11AN Epoxy adhesive features outstanding thermal conductivity. Superb electrical insulation properties. Tough bonds. High shear and peel strength. Cures at ambient temperatures. Low CTE. Paste viscosity. Serviceable from -100°F to +250°F. |
![]() |
Supreme 11ANHT High temperature resistant epoxy for bonding and sealing. Toughened formulation. Superior shear/peel strength. Excellent heat transfer properties. Superb dielectric characteristics, Serviceable from -112°F to +400°F. |