70 products match
![]() |
UV15X-6Med-2 UV curing system with high flexibility that is biocompatible per USP Class VI testing. Medium viscosity. Superior abrasion resistance. Non-yellowing. Reliable thermal and electrical insulator. Serviceable from -80°F to +250°F. |
![]() |
UV15X-6Med-2LV UV curing system with high flexibility that is biocompatible per ISO 10993-5. Medium viscosity. Superior abrasion resistance. Non-yellowing. Reliable thermal and electrical insulator. Serviceable from -80°F to +250°F. |
![]() |
UV16Med One part system, not oxygen inhibited, outstanding toughness and flexibility, can resist repeated autoclaving, passes ISO 10993-5 for cytotoxicity |
![]() |
UV17Med High flexibility and toughness. Outstanding abrasion resistance. Moderate viscosity. Resists thermal cycling and mechanical shocks. Bonds well to glass, metals, ceramics, composites and many plastics including polycarbonates, acrylics. Serviceable from -80°F to +250°F. |
![]() |
UV18Med USP Class VI and ISO 10993-5 approved system. Outstanding chemical and water resistance. Excellent electrical insulation properties. Rapid curing. Fast fixture times. Optically clear. Ideal for high production applications. Serviceable from -60°F to 250°F. |
UV18Med-2 ISO 10993-5 approved system. Outstanding chemical and water resistance. Excellent electrical insulation properties. Rapid curing. Fast fixture times. Low viscosity. Ideal for high production applications. Serviceable from -60°F to 250°F. |
|
![]() |
UV22DC80-1Med Dual cure system with UV and heat curing mechanisms. Cures at 80°C in shadowed out areas. Nano filled, high dimensional stability and abrasion resistance. Bonds well to metals, glass, ceramics and most plastics. Serviceable from -60°F to +350°F. |
UV26DCMed Specialty type UV curable adhesive with very fast curing time and high thermal stability. Its glass transition temperature is 160 to 170°C and its service temperature range is -60°F to +500°F. UV26DCMed passes ISO 10993-5 for cytotoxicity |
|
![]() |
X18Med Single component adhesive/primer for polyolefins. Cures at ambient temperatures. Very low viscosity. Easy to apply. Sets up in 30-45 minutes. Superb electrical insulator. Clear to light amber color. Serviceable from -60°F to +200°F. Passes ISO 10993-5 test. |
![]() |
X21Med Specially formulated one component system for bonding and priming polyolefinic surfaces. Can be used as a primer to promote adhesion of polyolefinic substrates to other surfaces such as metals, ceramics. Viscosit <250 cps. Room temperature curing. Serviceable from -60°F to +200°F. Passes ISO 10993-5 for medical devices. |