Two part, thermally conductive, electrically insulative epoxy for bonding and sealing featuring outstanding heat resistance; requires oven curing

EP46HT-1AO Two Part Epoxy Compound

Key Features

  • Impressive thermal conductivity and electrical insulation
  • High glass transition temperature
  • Excellent physical properties & dimensional stability
  • Meets MIL-STD-883J Section 3.5.2 for thermal stability
  • Meets NASA low outgassing specifications
  • Withstands 1,000 hours 85°C/85% RH