High temperature resistant, NASA low outgassing epoxy compound
Key Features
- Convenient handling, long working life
 - Cures rapidly at moderate temperatures
 - Superior bond strength properties
 - Widely used for its chemical resistance
 
Product Description
Master Bond EP62-1LO is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a very forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is greater than 12 hours. Typical cure schedules range from 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C. The cured epoxy resin exhibits remarkably high thermal stability with a glass transition temperature of 140-145°C. Also noteworthy is its outstanding chemical resistance to acids, bases, many solvents and other chemicals, even at elevated temperatures. This system has excellent electrical insulation properties. The color of Part A is clear and Part B is dark brown. EP62-1LO is primarily used as an adhesive, sealant and coating where the epoxy will be exposed to very aggressive conditions as well as where a long open time and NASA low outgassing are required.
Product Advantages
- Easy to use, very forgiving 100 to 10 mix ratio by weight (will fully cure using 100 to 5 mix ratio)
 - Superior resistance to a wide variety of chemicals, even at high temperatures
 - Service temperature range of -60°F to +450°F
 - Versatile cure schedules at various elevated temperatures
 - Excellent physical strength properties
 - Meets NASA low outgassing standards
 
Industrial Certifications
Packaging
EP62-1LO is available is various sizes and units to accommodate customer's needs.
			      