One component, non-corrosive silicone for bonding and sealing
Key Features
- Silver Filled, electrically conductive
 - Very low resistance
 - Room temperature curing
 - High temperature resistant
 
Product Description
Master Bond MasterSil 705S is an easy to use, one component, non-corrosive, electrically conductive, silver filled, silicone for bonding and sealing. The material is a gray colored paste. It cures readily at ambient temperatures when exposed to atmospheric moisture. MasterSil 705S features exceptionally low volume resistivity and is ideal for many electronic applications, especially those involving printed circuit boards. MasterSil 705S bonds well to a variety of substrates including metals, composites, many plastics and rubbers. It should be noted that it even adheres well to other silicone materials, a feature that enables it to be used with most gasketing materials. Its most outstanding physical properties are its high temperature resistance and flexibility, which allows it to withstand rigorous thermal cycling and thermal shocks. It is serviceable over the wide temperature range of -60°F to +400°F. Finally, MasterSil 705S can also be used in EMI/RFI shielding applications. It is most effective as an adhesive or sealant even when applied in thin sections. MasterSil 705S has wide applicability in electronic and electrical applications where low resistance combined with flexibility and high temperature resistance is desirable.
Packaging
MasterSil 705S is available is various sizes and units to accommodate customer's needs.
			      