Biocompatible. Pass USP Class VI and ISO cytotoxicity testing. Non-corrosive, neutral type curing system. Good sterilization resistance properties. Withstand rigorous thermal cycling. Elongation 250-350%. Volume resistivit >1015 ohm-cm. Tensile strength 700-1100psi.