Elastomeric Master Bond form-in-place gasketing materials feature low volume resisitivity, superior mechanical properties and resist aging degradation from high temperatures, humidity, fluids, dust and pressure. These formulations contain a wide range of special fillers such as silver, nickel, graphite, silver coated nickel particles to optimize EMI shielding effectiveness.
Moisture and thermal cure products exhibit high bond strength to plated metals, injection molded plastics and vacuum metalized surfaces. Resilient, non-corrosive, high tear strength compositions offer excellent compression set performance. Low modulus products absorb CTE mismatches. Conductive gasketing is designed to lower labor expenses, reduce raw material costs and shorten production cycle times. Applications range from automotive control systems to military electronics to medical electronic devices.
Master Bond’s Most Popular Electrically Conductive Form-in-Place Adhesives
|
MasterSil 705S Silver filled, one-part, no-mix, non-corrosive silicone system. Shore A hardness 70. Cures at room temperatures when exposed to atmospheric moisture. Extremely low volume resistivity. Most effective when applied in thin sections. |
|
|
MasterSil 973S-LO Silver filled, two part, addition cured type silicone. Excellent electrical conductivity. Passes NASA low outgassing test requirements. Highly flexible. Service temperature range from -120°F to +400°F. Volume resistivit >0.004 ohm-cm. |